FRP Flexural Strengthening design check for ACI PRC-440.2
Externally bonded FRP (carbon, glass or aramid; fabric or pre-cured laminate) on the soffit of an existing reinforced concrete beam or slab strip.
Create a free account to use it
7 days of the Professional plan, no card. After the trial the account moves to the Free plan; nothing is charged automatically.
What it checks
ACI PRC-440.2-17 Chapter 10 with debonding, the initial strain at installation, the strengthening limit, service.
Inputs
FRP Flexural Strengthening takes 14 inputs for the Australia and New Zealand code system, with the defaults below. Lengths are in m, forces in kN and stresses in MPa unless the unit column says otherwise.
| Input | Unit | Default |
|---|---|---|
| Existing section | ||
| Web width b (1000 for a slab strip) | mm | 1000 |
| Overall depth h | mm | 200 |
| Depth to the tension steel d | mm | 165 |
| Tension steel area A_s | mm² | 565 |
| Concrete strength f'c (in place) | MPa | 32 |
| Steel yield strength f_y | MPa | 500 |
| Moments | ||
| Service dead load moment M_D (present at installation) | kNm | 15 |
| Service live load moment M_L (new use) | kNm | 16 |
| Initial soffit strain ε_bi (0 = from the cracked section under M_D) | - | 0 |
| FRP system | ||
| FRP system Options: Carbon fabric laminate, wet lay-up: t_f 2.03 mm, f_fu* 883 MPa, ε_fu* 0.0090, E_f 97.9 GPa; Carbon fabric laminate, wet lay-up: t_f 1.0 mm, f_fu* 986 MPa, ε_fu* 0.0100, E_f 95.8 GPa; Carbon pre-cured laminate strip: t_f 1.2 mm, f_fu* 2800 MPa, ε_fu* 0.0170, E_f 165 GPa; Glass fabric laminate, wet lay-up: t_f 1.3 mm, f_fu* 575 MPa, ε_fu* 0.0220, E_f 26.1 GPa; Custom: enter the guaranteed properties of the product. | - | Carbon pre-cured laminate strip: t_f 1.2 mm, f_fu* 2800 MPa, ε_fu* 0.0170, E_f 165 GPa |
| Exposure (Table 9.4) Options: Interior; Exterior (bridges, parking structures, open structures); Aggressive (chemical plants, wastewater). | - | Exterior (bridges, parking structures, open structures) |
| FRP layout | ||
| Number of plies n | - | 1 |
| FRP width w_f | mm | 100 |
| Depth to the FRP d_f (h for the soffit) | mm | 200 |
Results and report
The module reports: FRP system; Design rupture strength f_fu = C_E f_fu*; Design rupture strain ε_fu; Debonding strain ε_fd; Initial strain ε_bi; FRP area A_f = n t_f w_f; Neutral axis depth c; Failure mode; Effective FRP strain ε_fe; FRP stress f_fe; Steel strain ε_s; Steel contribution M_ns.
It checks: Strengthened flexural strength: M_u ≤ φM_n; Existing tension steel A_s ≥ A_s,min.
Each module produces a report: numbered working, formulas with substituted values, tables and diagrams, ready to attach to a calculation package. The report carries a verification code that confirms it was made by TensorNode and has not been changed.
Example with the default inputs
FRP Flexural Strengthening with its default inputs for the Australia and New Zealand code system. The main inputs:
| Input | Value |
|---|---|
| Web width b (1000 for a slab strip) | 1000 mm |
| Overall depth h | 200 mm |
| Depth to the tension steel d | 165 mm |
| Tension steel area A_s | 565 mm² |
| Concrete strength f'c (in place) | 32 MPa |
| Steel yield strength f_y | 500 MPa |
| Service dead load moment M_D (present at installation) | 15 kNm |
| Service live load moment M_L (new use) | 16 kNm |
Headline results:
| Result | Value |
|---|---|
| FRP system | Carbon pre-cured laminate strip |
| Design rupture strength f_fu = C_E f_fu* | 2380.0 MPa |
| Design rupture strain ε_fu | 0.01445 |
| Debonding strain ε_fd | 0.00521 |
| Initial strain ε_bi | 0.00008 |
| FRP area A_f = n t_f w_f | 120 mm² |
Governing check: Strengthened flexural strength: M_u ≤ φM_n (ACI 440.2R-17 10.2.10, Eq. (10.2.10)), 43.6 kNm against 49.4 kNm, utilisation 0.88, passes.
Computed by TensorNode with the default inputs shown; a qualified engineer checks every result.
Design codes
FRP Flexural Strengthening works to 1 code system in United States. The standards and editions are listed below; clause numbers are cited in the report.
| Region | Standard and edition |
|---|---|
| United States | ACI PRC-440.2-17, ACI CODE-318-19 |
Use it in full during the 7-day trial of the Professional plan. Paid plans give access to the module packs. TensorNode is a calculation aid. Every result must be checked and accepted by a qualified engineer, who remains responsible for the design. Read the scope and limits of this module before you rely on a result.
Related modules
- Beam Shear
Reinforced-concrete beam shear to AS 3600 §8.2 - Beam Torsion
Reinforced-concrete beam torsion to AS 3600:2018 Cl. - Column Biaxial
RC column under axial load with biaxial bending to AS 3600 §10.6.3, the P-M interaction is built by strain compatibility about each axis, with reinforcement placed on all four faces (top/bottom bars resist X-axis bending, side bars resist Y-axis bending, both - Column Interaction
Rectangular reinforced-concrete column to AS 3600 §10 - Concrete Durability and Cover
Durability and cover to reinforcement to AS 3600:2018 Section 4 - Concrete Wall
RC wall in compression by the AS 3600 §11.5.3 simplified method - Corbel / Bracket
Reinforced-concrete corbel / bracket to AS 3600 - Crack Control
Crack control for RC beams/slabs by the AS 3600 §8.6.2.2 deemed-to-comply method
Open FRP Flexural Strengthening with a free account
7 days of the Professional plan, no card. After the trial the account moves to the Free plan; nothing is charged automatically.